The microstructure of compression molded Estane 5703 films exposed to 11%, 45%, and 80% relative humidity and 70 °C for 1 and 2 months has been studied by small-angle neutron scattering (SANS), Fourier transform infrared spectroscopy (FTIR), gel permeation chromatography (GPC), and differential scanning calorimetry (DSC). Scattering data indicated increase of the interdomain distance and domain size with a higher humidity and longer aging time. GPC data showed a progressive shortening of polyurethane chains with increasing humidity and aging time. The shortening of the polyurethane chains caused a drop of the glass transition temperature of soft segments, and promoted crystallization of the soft segments during long-time storage of the aged samples at room temperature. FTIR showed a substantial increase in the number of inter-urethane H-bonds in the aged samples. This correlates with the increase of the hard domain size and the degree of phase separation as measured by SANS. The data collected reveals that the reduced steric hindrance caused by hydrolysis of ester links in polybutylene adipate residues promotes the organization of hard segments into domains, leading to the increase of domain size and distance, as well as phase segregation in aged Estane. These findings provide insight into the effects of humidity and thermal aging on the microstructure of aged polyester urethane from molecular to nanoscale level.
Zobrazit více v PubMed
Prisacariu C. Polyurethane Elastomers: From Morphology to Mechanical Aspects. Springer Verlag; Wien, Austria: 2011.
Orler E.B., Wrobleski D.A., Smith M.E. Hydrolytic degradation of Estane 5703; Proceedings of the 22nd Aging, Compatibility and Stockpile Stewardship Conference; Oak Ridge, TN, USA. 27–30 April 1999.
Orler E.B., Wrobleski D.A., Cooke D.W., Bennett B.L., Smith M.E., Jahan M.S. Thermal Aging of Nitroplasticized Estane 5703. In Proceedings of the 24th Aging, Compatibility and Stockpile Stewardship Conference; Pantex, Amarillo, TX, USA. 29 April–3 May 2002.
Salazar M.R., Lightfoot J.M., Russell B.G., Rodin W.A., McCarty M., Wrobleski D.A., Orler E.B., Spieker D.A., Assink R.A., Pack R.T. Degradation of a poly(ester urethane) Elastomer. III. Estane 5703 Hydrolysis: Experiments and Modeling. J. Polym. Sci. Part A Polym. Chem. 2003;41:1136–1151. doi: 10.1002/pola.10656. DOI
Pierpoint S., Silverman J., Al-Sheikhly M. Effects of ionizing radiation on the aging of polyester based polyurethane binder. Radiat. Phys. Chem. 2001;62:163–169. doi: 10.1016/S0969-806X(01)00434-0. DOI
Fambri L., Penati A., Kolarik J. Synthesis and hydrolytic stability of model poly(ester urethane ureas) Angew. Makromol. Chem. 1995;228:201–219. doi: 10.1002/apmc.1995.052280116. DOI
Thompson D.G., Osborn J.C., Kober E.M., Schoonover J.R. Effects of hydrolysis-induced molecular weight changes on the phase separation of a polyester polyurethane. Polym. Degrad. Stab. 2006;91:3360–3370. doi: 10.1016/j.polymdegradstab.2006.05.019. DOI
Mang J.T., Peterson P.D., Orler E.B., Wrobleski D.A., Langlois D.A., Espada L.I., Hjelm R.P. Small-angle neutron scattering study of a thermally aged, segmented poly(ester urethane) binder. Neutron News. 2003;14:26–28. doi: 10.1080/10448630308218510. DOI
Espada L.I., Mang J.T., Orler E.B., Wrobleski D.A., Langlois D.A., Hjelm R.P. Structural characterization of segmented polyurethanes by small angle neutron scattering. MRS Proc. 2001;707 doi: 10.1557/PROC-707-AA10.11.1/DD11.11.1. DOI
Koberstein J.T., Galambos A.F., Leung L.M. Compression-molded polyurethane block copolymers. 1. Microdomain morphology and thermomechanical properties. Macromolecules. 1992;25:6195–6204. doi: 10.1021/ma00049a017. DOI
Krakovský I., Bubenikova Z., Urakawa H., Kajiwara K. Inhomogeneous structure of polyurethane networks based on poly(butadiene)diol: 1. The effect of the poly(butadiene) diol content. Polymer. 1997;38:3637–3643.
Krakovský I., Urakawa H., Kajiwara K. Inhomogeneous structure of polyurethane networks based on poly (butadiene) diol: 2. Time-resolved SAXS study of the microphase separation. Polymer. 1997;38:3645–3653.
Koberstein J.T., Russell T.P. Simultaneous SAXS-DSC study of multiple endothermic behavior in polyether-based polyurethane block copolymers. Macromolecules. 1986;19:714–720. doi: 10.1021/ma00157a039. DOI
Blundell D.J., Eeckhaut G., Fuller W., Mahendrasingam A., Martin C. Real time SAXS/stress–strain studies of thermoplastic polyurethanes at large strains. Polymer. 2002;43:5197–5207. doi: 10.1016/S0032-3861(02)00386-5. DOI
Mang J.T., Hjelm R.P., Orler E.B., Wrobleski D.A. Small-angle neutron scattering of a solvent-swollen segmented polyurethane as a probe of solvent distribution and polymer domain composition. Macromolecules. 2008;41:4358–4370. doi: 10.1021/ma800015g. DOI
Tian Q., Almásy L., Yan G., Sun G., Zhou X., Liu J., Rosta L., Chen B. Small-angle neutron scattering investigation of polyurethane aged in dry and wet air. Express Polym. Lett. 2014;8:345–351.
Keiderling U. The new “BerSANS-PC” software for reduction and treatment of small angle neutron scattering data. Appl. Phys. A. 2002;74:s1455–s1457. doi: 10.1007/s003390201561. DOI
Breßler I., Kohlbrecher J., Thünemann A.F. SASfit: A tool for small-angle scattering data analysis using a library of analytical expressions. J. Appl. Cryst. 2015;48:1587–1598. doi: 10.1107/S1600576715016544. PubMed DOI PMC
Debye P., Anderson R., Brumberger H. Scattering by an inhomogeneous solid. II. The correlation function and its application. J. Appl. Phys. 1957;28:679–683.
Linliu K., Chen S.A., Yu T.L., Lin T.L., Lee C.H., Kai J.J., Chang S.L., Lin J.S. A small-angle X-ray scattering study of microphase separation transition of polyurethanes: Effect of hard segments. J. Polym. Res. 1995;2:63–70. doi: 10.1007/BF01493435. DOI
Tian Q., Takács E., Krakovský I., Horváth Z.E., Rosta L., Almásy L. Study on the microstructure of polyester polyurethane irradiated in air and water. Polymers. 2015;7:1755–1766.
Coleman M.M., Lee H.H., Skrovanek D.J., Painter P.C. Hydrogen bonding in polymers. 4. Infrared temperature studies of a simple polyurethane. Macromolecules. 1986;19:2149–2157. doi: 10.1021/ma00162a008. DOI
Coleman M.M., Skrovanek D., Hu J., Painter P.C. Hydrogen bonding in polymer blends. 1. FTIR studies of urethane-ether blends. Macromolecules. 1988;21:59–65. doi: 10.1021/ma00179a014. DOI
Luo N., Wang D.N., Ying S.K. Hydrogen-Bonding properties of segmented polyether poly(urethane urea) copolymer. Macromolecules. 1997;30:4405–4409. doi: 10.1021/ma951386e. DOI
Nierzwicki W., Majewska Z. Swelling properties of urethane elastomers and their bearing on microphase separation. J. Appl. Polym. Sci. 1979;24:1089–1099. doi: 10.1002/app.1979.070240421. DOI
Yanagihara Y., Osak N., Murayama S., Saito H. Thermal annealing behavior and structure development of crystalline hard segment domain in a melt-quenched thermoplastic polyurethane. Polymer. 2013;54:2183–2189. doi: 10.1016/j.polymer.2013.02.005. DOI
Li X., Stribeck A., Schulz I., Pöselt E., Eling B., Hoell A. Nanostructure of thermally aged thermoplastic polyurethane and its evolution under strain. [(Accessed on 14 May 2016)];Eur. Polym. J. 2015 doi: 10.1016/j.eurpolymj.2015.11.027. Available online: DOI
Princi E., Vicini S., Stagnaro P., Conzatti L. The nanostructured morphology of linear polyurethanes observed by transmission electron microscopy. Micron. 2011;42:3–7. doi: 10.1016/j.micron.2010.09.007. PubMed DOI
Gardner R.J., Martin J.R. Effect of relative humidity on the mechanical properties of poly (1,4-butylene terephthalate) J. Appl. Polym. Sci. 1980;25:2353–2361. doi: 10.1002/app.1980.070251021. DOI
Vermette P., Griesser H.J., Laroche G., Guidoin R. Biomedical Applications of Polyurethanes. Landes Bioscience; Georgetown, TX, USA: 2001.
Schoonover J.R., Thompson D.G., Osborn J.C., Orler E.B., Wrobleski D.A., Marsh A.L., Wang H., Ralmer R.A. Infrared linear dichroism study of a hydrolytically degraded poly(ester urethane) Polym. Degrad. Stab. 2001;74:87–96. doi: 10.1016/S0141-3910(01)00105-7. DOI
Li Y., Gao T., Liu J., Linliu K., Desper C.R., Chu B. Multiphase structure of a segmented polyurethane: Effects of temperature and annealing. Macromolecules. 1992;25:7365–7372. doi: 10.1021/ma00052a045. DOI