Comparison of properties of tablets and energy profile of compaction of two spray-dried lactoses
J. Muzíková, P. Sináglová,
Language English Country Poland
Document type Comparative Study, Journal Article, Research Support, Non-U.S. Gov't
NLK
Free Medical Journals
from 1998
ROAD: Directory of Open Access Scholarly Resources
from 1998
PubMed
23610968
Knihovny.cz E-resources
- MeSH
- Aerosols MeSH
- Cellulose chemistry MeSH
- Chemistry, Pharmaceutical MeSH
- Technology, Pharmaceutical methods MeSH
- Kinetics MeSH
- Stearic Acids chemistry MeSH
- Lactose chemistry MeSH
- Lubricants chemistry MeSH
- Tensile Strength MeSH
- Compressive Strength MeSH
- Excipients chemistry MeSH
- Solubility MeSH
- Tablets MeSH
- Desiccation MeSH
- Publication type
- Journal Article MeSH
- Research Support, Non-U.S. Gov't MeSH
- Comparative Study MeSH
The paper compared two spray-dried lactoses Flowlac 100 and SuperTab 14SD from the standpoint of tensile strength and disintegration time of tablets, the effect of an addition of the lubricant magnesium stearate and silicified microcrystalline cellulose on these properties, and also from the standpoint of the energy profile of compression. The comparison of the values was performed at the compression force of 15 kN. The strength of tablets was higher in the case of SuperTab 14SD, an increase in the concentration of magnesium stearate did not decrease tablet strength. Prosolv SMCC 90 increased the strength of tablets and made it equal for both lactoses, but it also increased the sensitivity to the added lubricant. The disintegration time of tablets was shorter in the case of SuperTab 14SD, an increased concentration of magnesium stearate prolonged it, and an addition of Prosolv SMCC 90 shortened it and made it equal for both lactoses. From the energy standpoint, the maximal energy was higher in the case of SuperTab 14SD, an addition of Prosolv SMCC 90 increased it and again made it equal for both lactoses. The differences in the values of the maximal energy were primarily due to the values of the energy for friction and the energy accumulated by the tablet after compression, and there was no marked difference in the values of the energy of decompression. SuperTab 14SD showed a higher plasticity than Flowlac 100.
- 000
- 00000naa a2200000 a 4500
- 001
- bmc13023921
- 003
- CZ-PrNML
- 005
- 20130704095551.0
- 007
- ta
- 008
- 130703s2013 pl f 000 0|eng||
- 009
- AR
- 035 __
- $a (PubMed)23610968
- 040 __
- $a ABA008 $b cze $d ABA008 $e AACR2
- 041 0_
- $a eng
- 044 __
- $a pl
- 100 1_
- $a Muzíková, Jitka $u Department of Pharmaceutical Technology, Charles University in Prague, Faculty of Pharmacy in Hradec Králové, Czech Republic. muzikova@faf.cuni.cz
- 245 10
- $a Comparison of properties of tablets and energy profile of compaction of two spray-dried lactoses / $c J. Muzíková, P. Sináglová,
- 520 9_
- $a The paper compared two spray-dried lactoses Flowlac 100 and SuperTab 14SD from the standpoint of tensile strength and disintegration time of tablets, the effect of an addition of the lubricant magnesium stearate and silicified microcrystalline cellulose on these properties, and also from the standpoint of the energy profile of compression. The comparison of the values was performed at the compression force of 15 kN. The strength of tablets was higher in the case of SuperTab 14SD, an increase in the concentration of magnesium stearate did not decrease tablet strength. Prosolv SMCC 90 increased the strength of tablets and made it equal for both lactoses, but it also increased the sensitivity to the added lubricant. The disintegration time of tablets was shorter in the case of SuperTab 14SD, an increased concentration of magnesium stearate prolonged it, and an addition of Prosolv SMCC 90 shortened it and made it equal for both lactoses. From the energy standpoint, the maximal energy was higher in the case of SuperTab 14SD, an addition of Prosolv SMCC 90 increased it and again made it equal for both lactoses. The differences in the values of the maximal energy were primarily due to the values of the energy for friction and the energy accumulated by the tablet after compression, and there was no marked difference in the values of the energy of decompression. SuperTab 14SD showed a higher plasticity than Flowlac 100.
- 650 _2
- $a aerosoly $7 D000336
- 650 _2
- $a celulosa $x chemie $7 D002482
- 650 _2
- $a farmaceutická chemie $7 D002626
- 650 _2
- $a pevnost v tlaku $7 D019245
- 650 _2
- $a vysoušení $7 D003890
- 650 _2
- $a pomocné látky $x chemie $7 D005079
- 650 _2
- $a kinetika $7 D007700
- 650 _2
- $a laktosa $x chemie $7 D007785
- 650 _2
- $a lubrikanty $x chemie $7 D054327
- 650 _2
- $a rozpustnost $7 D012995
- 650 _2
- $a kyseliny stearové $x chemie $7 D013229
- 650 _2
- $a tablety $7 D013607
- 650 _2
- $a farmaceutická technologie $x metody $7 D013678
- 650 _2
- $a pevnost v tahu $7 D013718
- 655 _2
- $a srovnávací studie $7 D003160
- 655 _2
- $a časopisecké články $7 D016428
- 655 _2
- $a práce podpořená grantem $7 D013485
- 700 1_
- $a Sináglová, Pavla $u -
- 773 0_
- $w MED00000128 $t Acta poloniae pharmaceutica $x 0001-6837 $g Roč. 70, č. 1 (2013), s. 129-35
- 856 41
- $u https://pubmed.ncbi.nlm.nih.gov/23610968 $y Pubmed
- 910 __
- $a ABA008 $b sig $c sign $y a $z 0
- 990 __
- $a 20130703 $b ABA008
- 991 __
- $a 20130704100010 $b ABA008
- 999 __
- $a ok $b bmc $g 987601 $s 822301
- BAS __
- $a 3
- BAS __
- $a PreBMC
- BMC __
- $a 2013 $b 70 $c 1 $d 129-35 $i 0001-6837 $m Acta poloniae pharmaceutica $n Acta Pol Pharm $x MED00000128
- LZP __
- $a Pubmed-20130703